不同改性處理對橡膠木抗菌性能影響研究
中圖分類號:S794.1 文獻(xiàn)標(biāo)識碼:A DOI: 10.7525/j.issn.1006-8023.2025.04.014
Abstract:Usingrubberwoodasrawmaterial,orthogonal experimentaldesign wasused to exploretheinfluenceof silverloaded nano itanium dioxide impregnated heat treatmentonthe mold and corrosionresistance of rubberwood,and compared themold and corrosion resistance,dryshrinkage and wet swelling properties ofthe control timber,heat-treated timber,silver-loadednano titanium dioxide impregnatedtimberandsilver-loaded nano titaniumdioxideimpregnated heat-treated timber,andtheinfluence mechanismof diferent modification treatments onthe physicochemical properties of the timber wasrevealedthrough the means of electron microscopy,XRD(X-ray difraction).Theresults showed that the optimal process of silver-loaded nano titanium dioxide impregnated heat treatment was 16O C,2.5 h,1. 5% silver loading,1.5mg/mL modifierconcentration,6O min vacuum impregnation time,atthis time,the modified timber had thegreatest efficacy inthe preventionofAspergillusnigerandPenicilliumcitrinum,both of them were 100% ,and the modified timberhadthe smallestrateofqualitylossunderthe influenceof white-rotfungus and brown-rotfungus,which were 2.36% and1.9 % ,respectively. Compared with the control timber,heat-treated timber and silver-loaded nano titaniumdioxide impregnated timber,silver-loaded nano titanium dioxide impregnated heat-treated timber hadthelowest wetswellng anddryshrinkage,theradial,tangentialand volumetric water-absorbing wetswellingrate was reduced by 31. 34% -36. 36% compared with that of the control timber,the radial,tangential and volumetric moisture-absorbing wet swelling rate was reduced by 41. 06% -61. 7% compared with that of the control timber,the radial, tangential and volumetric air-drying dry shrinkage rate was reduced by up to 23.28%-32. 24% compared with that of the control timber.
Thesilver-loadednanotitaniumdioxideimpregnatedheat treatmentcanrealizetheuniformloadingofsilver-loaded nano titanium dioxideparticles in wood,which cancomprehensively improvethe moldand corrosionresistance and dimensional stability of wood,and realize the excellent wood modification effect.
Keywords:Silver-loaded nano titanium dioxide;heat treatment;mold and corrosion resistance;wet swelling proper ties;wood modification
0 引言
橡膠木(Heveabrasiliensis)作為一種重要的熱帶木材,因其生長迅速、紋理美觀和易于加工等特性而被廣泛應(yīng)用于家具、建筑和裝飾等領(lǐng)域1。(剩余14232字)
- 大興安嶺寒溫帶針葉林群落特征及...
- 解除休眠水曲柳種子的超干貯藏研...
- 快速升溫和升溫間歇期興安落葉松...
- 不同徑級紅松生長對氣候變化響應(yīng)...
- 基于硼化學(xué)串聯(lián)糖結(jié)晶體系分離高...
- 二氧化硅包裹銳鈦礦型二氧化鈦處...
- 聚乙二醇處理對杞柳軟化效果的影...
- 不同厚度中密度纖維板的孔隙分形...
- 刀狀黑黃檀木材解剖結(jié)構(gòu)及其密度...
- 基于改進(jìn)YOLOv8模型的木材...
- 基于改進(jìn)型YOLOv8的木材缺...
- 基于改進(jìn)YOLOv8的膠合板單...
- 基于聲發(fā)射信號多重分形特征的櫸...
- 不同改性處理對橡膠木抗菌性能影...
- 基于改進(jìn)YOLOv5s的松科球...
- 中密度纖維板板壞密度與含水率對...
- 基于離散元法的生物質(zhì)熱解螺旋抄...
- 基于非支配遺傳算法-Ⅱ的放大電...
- 深紋核桃側(cè)枝搖振采摘振動參數(shù)...
- 基于視覺檢測的膠合板表面缺陷修...