熱軋帶鋼跑偏原因分析及控制措施
摘 要:針對(duì)某1 250 mm熱連軋生產(chǎn)線在精軋機(jī)軋制時(shí)經(jīng)常出現(xiàn)帶鋼跑偏軋破、軋廢的現(xiàn)象,從溫度控制、粗軋板形控制、軋輥不均勻磨損、軋輥冷卻水、軋制潤(rùn)滑、軋機(jī)間隙、設(shè)備對(duì)中等方面進(jìn)行逐一排查整改,最終將跑偏降級(jí)軋廢控制在合理范圍內(nèi)。
關(guān)鍵詞:熱軋帶鋼;跑偏;對(duì)中;潤(rùn)滑;間隙
ANALYSIS AND CONTROL MEASURES OF RUNNING DEVIATION OF HOT STRIP
Li Aibin Yang Shaodong Song Huadong
(Guangxi Shenglong Metallurgical Co., Ltd Fangchenggang 538000,China)
Abstract:In this paper, a 1 250 mm hot continuous rolling production line in the finishing mill often occurred strip deviation rolling broken, The phenomenon of rolling waste is checked and rectified one by one from the aspects of temperature control, rough rolling shape control, roll uneven wear, roll cooling water, rolling lubrication, rolling mill gap and equipment, and finally the running deviation and demotion rolling waste is controlled within a reasonable range.
Key Words: hot strip misalignment lubrication clearance
0 引 言
某1 250 mm熱軋帶鋼生產(chǎn)線2011年11月投產(chǎn),主要以生產(chǎn)冷軋基料SPHC、Q195厚度3.0 mm為主,從2018年10月開(kāi)始精軋機(jī)軋制跑偏軋破、軋廢居高不下,統(tǒng)計(jì)顯示平均每月因跑偏軋破降級(jí)品占總降級(jí)品的20%,跑偏廢鋼占總廢鋼的30%。(剩余2459字)
-
-
- 冶金信息導(dǎo)刊
- 2024年04期
- 我國(guó)首個(gè)省級(jí)冶金工業(yè)園區(qū)下屬經(jīng)...
- 二十冶資產(chǎn)證券化產(chǎn)品發(fā)行情況及...
- 我國(guó)重點(diǎn)黃金企業(yè)恒邦股份的經(jīng)營(yíng)...
- 質(zhì)量監(jiān)督方法創(chuàng)新實(shí)現(xiàn)質(zhì)量管理提...
- 基于相變熱模擬方法的工藝調(diào)控對(duì)...
- 污染土壤修復(fù)技術(shù)對(duì)比分析及應(yīng)用...
- 輥縫標(biāo)零技術(shù)在型鋼軋機(jī)上的應(yīng)用...
- 直讀光譜儀測(cè)定高碳鋼中碳元素偏...
- SPA-H強(qiáng)度偏低分析與研究...
- 一種無(wú)花鍍鋅板典型漏鍍?nèi)毕莸姆?..
- 本鋼板材煉鋼廠脫磷效率的研究...
- 熱軋帶鋼跑偏原因分析及控制措施...
- 熱軋供冷軋高強(qiáng)鋼基料頭部板形控...
- 濕法脫硫漿液制備設(shè)施的創(chuàng)新與應(yīng)...
- 密封閥軸端密封結(jié)構(gòu)分析...
- 德國(guó)鋼鐵工業(yè)發(fā)展及啟示分析...
- 習(xí)近平文化思想引領(lǐng)中文科技期刊...